After calcination to remove the underlying latex, free-standing silica shells were obtained. ... In the coatings prepd. using 10 wt% colloidal silica, as the content of colloidal silica added increased to 8 g, 16 g, 24 g, and 40 g, the WCA of the coating decreased to 56°, 37°, 10°, and 5°, resp. From this result, it can be seen that a ...Web