Adding CDW aggregate led to a decrease of compressive strength by 12 and 25 %, when 25–30% [11,12] or 100 % NA was substituted by CDW aggregate [13,14,15]. However, no significant effect was seen when the coarse or fine recycled aggregate was applied to substitute up to 30 % of coarse NA [16,17,18,19,20] or 20 % of fine NA .Web