test. The CSK samples were crushed to 3–5 mm using a jaw crusher and then ground in a ball mill. After grinding, the material was sieved with a standard 200-mesh sieve, and the sieved material was readded to the ball mill. The particle size of CSK after grinding is d50 = 53.28 m. Subsequently, the ground product was encapsulated in nylon …Web